I wanted to inquire about the material used for this little knife. I picked it up in a bundled deal unknowing of the brand stamp. The seller wasn't sure due to the pitting around the tang stamps.
As you can see from the pictures there is some shrinkage of the scales and minor hairline cracking. But overall very clean.
So my question is has anyone else here have a similar knife with this material, and if so is there a problem with out gassing? I can not find any rust or issues associated with the effects other than the pitting.
I didn't pay much for it, so not a high value loss if its going south... it still has great snap and no play.
Appreciate the feedback and any other details you may be able to help with.
Merry Christmas y'all, Randy
I wanted to inquire about the material used for this little knife. I picked it up in a bundled deal unknowing of the brand stamp. The seller wasn't sure due to the pitting around the tang stamps.
As you can see from the pictures there is some shrinkage of the scales and minor hairline cracking. But overall very clean.
So my question is has anyone else here have a similar knife with this material, and if so is there a problem with out gassing? I can not find any rust or issues associated with the effects other than the pitting.
I didn't pay much for it, so not a high value loss if its going south... it still has great snap and no play.
Appreciate the feedback and any other details you may be able to help with.
Merry Christmas y'all, Randy
- peanut740
- Gold Tier

- Posts: 8133
- Joined: Fri Jan 23, 2009 2:32 pm
- Location: Ohio, along the river
- Contact:
- TPK
- Posts: 11024
- Joined: Sun Mar 31, 2019 6:16 pm
- Location: Bayern, Germany
- Contact:
Re: Western States pearl composition whittler
Cool looking knife with a cool stamp Randy!
TOM - KGFG - (Knife-Guy-From-Germany)
I believe..., every knife is a soul, looking for a soulmate.
Weebit-Nano https://www.weebit-nano.com/
https://en.m.wikipedia.org/wiki/Weebit_Nano
US - ARMY - COMBAT - ENGINEERS - 1990 - 1993 - God Bless Our Troops!
I believe..., every knife is a soul, looking for a soulmate.
Weebit-Nano https://www.weebit-nano.com/
https://en.m.wikipedia.org/wiki/Weebit_Nano
US - ARMY - COMBAT - ENGINEERS - 1990 - 1993 - God Bless Our Troops!
-
kootenay joe
- Posts: 13373
- Joined: Mon Jan 11, 2016 5:36 pm
- Location: West Kootenays, B.C.
Re: Western States pearl composition whittler
Some people call this "Cracked Ice" celluloid even though it is not white like pearl that it imitates. It is a celluloid that seems to last longer than many other celluloids. From the shrinkage you can tell it has off gassed a little. It could stay like this for years or continue to break down.
kj
kj
- edge213
- Gold Tier

- Posts: 8502
- Joined: Sat Jan 25, 2014 12:48 am
- Location: The Crossroads of America
Re: Western States pearl composition whittler
First, this is not a disagreement with what you said.kootenay joe wrote: ↑Wed Dec 23, 2020 9:19 pm Some people call this "Cracked Ice" celluloid even though it is not white like pearl that it imitates. It is a celluloid that seems to last longer than many other celluloids. From the shrinkage you can tell it has off gassed a little. It could stay like this for years or continue to break down.
kj
"From the shrinkage you can tell it has off gassed a little ".
I have seen a lot of celluloid that shows some shrinkage, but no other signs of outgassing. I seems to me it can shrink a little without actually outgassing.
What say you?
David
"Glowing like the metal on the edge of a knife" Meat Loaf
"Glowing like the metal on the edge of a knife" Meat Loaf
-
Gunsil
- Posts: 3082
- Joined: Fri Feb 28, 2014 5:25 pm
- Location: Lower Hudson River valley, N.Y.
Re: Western States pearl composition whittler
I agree that this type of cell is often pretty stable and I agree that celluloid can shrink without outgassing.
- Ripster
- Silver Tier

- Posts: 5051
- Joined: Tue Apr 07, 2020 6:37 pm
- Location: Wi.USA
Re: Western States pearl composition whittler
Hey Randy ,if you don’t want to remove the handles, then store in dry place, out of the sun . That’s what I was told ,so my old advertising knives , with 2or 3 digit phone numbers is what I’ve done over the years. They’ve held up okay,still wouldn’t trust it enough to store with any that are valuable. It can outgas in no time once it starts.
There are some good posts here atAAPK regarding celluloid material.
Take care ,stay safe . MERRY CHRISTMAS/ HAPPY HOLIDAYS.
There are some good posts here atAAPK regarding celluloid material.
Take care ,stay safe . MERRY CHRISTMAS/ HAPPY HOLIDAYS.
JP
-
Gone2Three
- Bronze Tier

- Posts: 758
- Joined: Thu Mar 19, 2020 5:32 am
Re: Western States pearl composition whittler
-
Gone2Three
- Bronze Tier

- Posts: 758
- Joined: Thu Mar 19, 2020 5:32 am
Re: Western States pearl composition whittler
Appreciate the excellent information gentlemen, I've seen some pretty ugly out gassing casualties posted here. That's why I was asking, it didn't seem like the others with major rusting and all.
The pitting and minor shrinkage are the only visual queues.
With that said, I'll make sure to keep it with my other celluloid friends
Thanks
The pitting and minor shrinkage are the only visual queues.
With that said, I'll make sure to keep it with my other celluloid friends
Thanks
- tongueriver
- Posts: 7242
- Joined: Tue Sep 16, 2008 8:01 pm
Re: Western States pearl composition whittler
I have owned some WESTERN knives with this cracked ice celluloid and I can tell you that it does indeed gas and cause rusting of the steel in the vicinity. It is not a good risk as cracked ice from other makers go.
-
kootenay joe
- Posts: 13373
- Joined: Mon Jan 11, 2016 5:36 pm
- Location: West Kootenays, B.C.
Re: Western States pearl composition whittler
By what means does it shrink if not by out gassing ?
I think this needs an organic chemist to answer. It is not shrinking from loss of moisture but it has to undergo some chemical reaction to cause it to loose volume.
The pre-Delrin 'plastics' used for knife handles can shrink greatly but these are not off gassing. There must be some chemical reaction that causes the molecular structure to react and re-arrange itself into something that takes up less space. It was the search for a stable plastic that does not shrink that lead to the invention of Delrin.
kj
-
Gone2Three
- Bronze Tier

- Posts: 758
- Joined: Thu Mar 19, 2020 5:32 am
Re: Western States pearl composition whittler
Very interesting topic, and this is why I asked here on the fourm. I've avoided investing in celluloid material knives just for this particular reason.kootenay joe wrote: ↑Thu Dec 24, 2020 1:24 amBy what means does it shrink if not by out gassing ?
I think this needs an organic chemist to answer. It is not shrinking from loss of moisture but it has to undergo some chemical reaction to cause it to loose volume.
The pre-Delrin 'plastics' used for knife handles can shrink greatly but these are not off gassing. There must be some chemical reaction that causes the molecular structure to react and re-arrange itself into something that takes up less space. It was the search for a stable plastic that does not shrink that lead to the invention of Delrin.
kj
I own about 6 that I keep separate from the collection. About half were purchased prior to joining here, now I'm weary or just paranoid about having them around
- zzyzzogeton
- Posts: 1842
- Joined: Tue Jun 20, 2017 8:47 pm
- Location: In the Heart of Texas on the Blackland Prairie
Re: Western States pearl composition whittler
Just an aside --- Western NEVER called it "cracked ice".
Western's advertising spiel was "Composition Pearl" or "Pearl Composition".
This is a 2363T, made in 1941. The sheeps foot blade is a post-sale modification. The knife was also made as the 2363TF, with a nail file in place of one of the smaller pen knife blades.
This specific model was not revived after WW2. The leading 2 indicates Pearl Composition. The first 3 indicates the number of blades. The 63 is the pattern, an equal end pen knife. The trailing T indicated the knife has "tip bolsters", skinny little bolsters on the tip of the handles.
Western's advertising spiel was "Composition Pearl" or "Pearl Composition".
This is a 2363T, made in 1941. The sheeps foot blade is a post-sale modification. The knife was also made as the 2363TF, with a nail file in place of one of the smaller pen knife blades.
This specific model was not revived after WW2. The leading 2 indicates Pearl Composition. The first 3 indicates the number of blades. The 63 is the pattern, an equal end pen knife. The trailing T indicated the knife has "tip bolsters", skinny little bolsters on the tip of the handles.
-
Gone2Three
- Bronze Tier

- Posts: 758
- Joined: Thu Mar 19, 2020 5:32 am
Re: Western States pearl composition whittler
Wow, thanks!...I couldn't find anything whatsoever on my search originally except the name of the material as stated in my title.zzyzzogeton wrote: ↑Thu Dec 24, 2020 2:44 am Just an aside --- Western NEVER called it "cracked ice".
Western's advertising spiel was "Composition Pearl" or "Pearl Composition".
This is a 2363T, made in 1941. The sheeps foot blade is a post-sale modification. The knife was also made as the 2363TF, with a nail file in place of one of the smaller pen knife blades.
This specific model was not revived after WW2. The leading 2 indicates Pearl Composition. The first 3 indicates the number of blades. The 63 is the pattern, an equal end pen knife. The trailing T indicated the knife has "tip bolsters", skinny little bolsters on the tip of the handles.
I really appreciate the information on this particular knife
- 1967redrider
- Gold Tier

- Posts: 21571
- Joined: Wed Feb 02, 2011 4:23 pm
- Location: Alexandria, VA
- Contact:
Re: Western States pearl composition whittler
I was looking at a 4 line Camillus utility knife with black (comp?) scales, and they shrank much like a fur hide would with none of the out-gassing corrosiveness. It just shrank like a drum stretched taught by the pins. So I think certain materials can shrink without bombing out the blades and liners.
M other
O f
T oilet
S eat
is a play on the real Mother Of Pearl handle material.
M other
O f
T oilet
S eat
is a play on the real Mother Of Pearl handle material.
Pocket, fixed, machete, axe, it's all good!
You're going to look awfully silly with that knife sticking out of your @#$. -Clint Eastwood, High Plains Drifter
CHRIST IS KING
You're going to look awfully silly with that knife sticking out of your @#$. -Clint Eastwood, High Plains Drifter
CHRIST IS KING
-
Gone2Three
- Bronze Tier

- Posts: 758
- Joined: Thu Mar 19, 2020 5:32 am
Re: Western States pearl composition whittler
1967redrider wrote: ↑Thu Dec 24, 2020 2:59 am I was looking at a 4 line Camillus utility knife with black (comp?) scales, and they shrank much like a fur hide would with none of the out-gassing corrosiveness. It just shrank like a drum stretched taught by the pins. So I think certain materials can shrink without bombing out the blades and liners.
M other
O f
T oilet
S eat
is a play on the real Mother Of Pearl handle material.![]()
I've got more than a few of these comp handle knives myself, one of which is also a 4 line camillus camp knife. It's a solid old knife, just has some shrinking of the scales like the others I've seen.
-
kootenay joe
- Posts: 13373
- Joined: Mon Jan 11, 2016 5:36 pm
- Location: West Kootenays, B.C.
Re: Western States pearl composition whittler
I too have a few of the Camillus knives with jigged black plastic that has shrunk ++. It's not celluloid because blades/bolsters are not stained or corroded. Delrin came into use in 1960 so these knives are likely 1950's ?
kj
kj
-
knife7knut
- Posts: 10697
- Joined: Tue Nov 06, 2007 9:02 pm
- Location: Tecumseh,Michigan
Re: Western States pearl composition whittler
I have a theory about why certain colors of celluloid seem to be more prone to outgassing or degradation or whatever you wish to call it.
Although not a hard and fast rule the ones that seem to deteriorate the most are clear handles and the "cracked ice" versions that are mostly white in color. When I was working in a body shop back in the early 1970's we had a lot of problems with clear coatings(which were just starting to be used extensively on factory finishes)deteriorating badly in a relatively short time.
Before they started using the newer acrylic finishes which are for the most part crystal clear,the nitrocellulose clears always had a bit of yellow toner added to them to make them more stable.They did eventually deteriorate but it took a much longer period of time to start.
As celluloid is composed of the same basic materials as nitrocellulose lacquer,it also seems to work in the same manner:clear and white handles seem to go faster than ones with a yellowish tint and other colors.As for the shrinkage problem,that is part of the drying process.As celluloid is essentially nitrocellulose fiber,camphor,and alcohol the first component is the evaporation of the alcohol followed I would think by the camphor. The rate at which these chemicals are lost may or may not be dependent on whether the proper mixture was done at the time of manufacture.Even a slight variance in composition could cause a drastic change.
Newer acrylic products such as paints have other problems to deal with.Two part paints(base and catalyst)depend on a precise mixture of components to effect a proper cure.Too much or too little of one or the other can cause it to never cure or cure too rapidly and not adhere properly. Another factor is temperature.If a two part coating is applied on too cold a surface(usually under 40 degreesF) or it is left out in the cold the top layer may cure but it will remain soft indefinitely. DO NOT ask me how I know this!
Anyway that is my take on out-gassing for what it's worth.
Although not a hard and fast rule the ones that seem to deteriorate the most are clear handles and the "cracked ice" versions that are mostly white in color. When I was working in a body shop back in the early 1970's we had a lot of problems with clear coatings(which were just starting to be used extensively on factory finishes)deteriorating badly in a relatively short time.
Before they started using the newer acrylic finishes which are for the most part crystal clear,the nitrocellulose clears always had a bit of yellow toner added to them to make them more stable.They did eventually deteriorate but it took a much longer period of time to start.
As celluloid is composed of the same basic materials as nitrocellulose lacquer,it also seems to work in the same manner:clear and white handles seem to go faster than ones with a yellowish tint and other colors.As for the shrinkage problem,that is part of the drying process.As celluloid is essentially nitrocellulose fiber,camphor,and alcohol the first component is the evaporation of the alcohol followed I would think by the camphor. The rate at which these chemicals are lost may or may not be dependent on whether the proper mixture was done at the time of manufacture.Even a slight variance in composition could cause a drastic change.
Newer acrylic products such as paints have other problems to deal with.Two part paints(base and catalyst)depend on a precise mixture of components to effect a proper cure.Too much or too little of one or the other can cause it to never cure or cure too rapidly and not adhere properly. Another factor is temperature.If a two part coating is applied on too cold a surface(usually under 40 degreesF) or it is left out in the cold the top layer may cure but it will remain soft indefinitely. DO NOT ask me how I know this!
Anyway that is my take on out-gassing for what it's worth.